Atomic Layer Deposition of LithiumâNickelâSilicon Oxide Cathode Material for Thin-Film Lithium-Ion Batteries
Maximov, Maxim, Nazarov, Denis, Rumyantsev, Aleksander, Koshtyal, Yury, Ezhov, Ilya, Mitrofanov, Ilya, Kim, Artem, Medvedev, Oleg, Popovich, AnatolyVolume:
13
Journal:
Energies
DOI:
10.3390/en13092345
Date:
May, 2020
Fichier:
PDF, 7.98 MB
2020