Nano-indentation investigation on the local softening of equiaxed zone in 2060-T8/2099-T83 aluminum-lithium alloys T-joints welded by double-sided laser beam welding
Han, Bing, Chen, Yanbin, Tao, Wang, Lei, Zhenglong, Li, Hao, Guo, Shu, Li, PengVolume:
756
Langue:
english
Journal:
Journal of Alloys and Compounds
DOI:
10.1016/j.jallcom.2018.05.014
Date:
August, 2018
Fichier:
PDF, 9.41 MB