ChemInform Abstract: EFFECT OF SULFUR DIOXIDE AND PH ON THE ANODIC BEHAVIOR AND PITTING CORROSION OF ALLOY 600
BERGE, PH., JOVANCICEVIC, V., NOEL, D., SAINT-PAUL, P.Volume:
14
Journal:
Chemischer Informationsdienst
DOI:
10.1002/chin.198306030
Date:
February, 1983
Fichier:
PDF, 207 KB
1983