Low cycle fatigue performance of Ni-based superalloy coated with complex thermal barrier coating
Šulák, Ivo, Obrtlík, Karel, Čelko, Ladislav, Chráska, Tomáš, Jech, David, Gejdoš, PavelVolume:
139
Langue:
english
Journal:
Materials Characterization
DOI:
10.1016/j.matchar.2018.03.023
Date:
May, 2018