Methanol electro-oxidation on Pt nanocatalysts prepared by atomic layer deposition
Hsieh, Chien-Te, Tzou, Dong-Ying, Jiang, Mei-TingVolume:
794
Langue:
english
Journal:
Journal of Electroanalytical Chemistry
DOI:
10.1016/j.jelechem.2017.04.020
Date:
June, 2017
Fichier:
PDF, 1.51 MB