A Comparison of the Plastic-Flow Response of a Powder-Metallurgy Nickel-Base Superalloy Under Nominally-Isothermal and Transient-Heating Hot-Working Conditions
Semiatin, S. L., Mahaffey, D. W., Tung, D. J., Zhang, W., Senkov, O. N.Volume:
48
Langue:
english
Journal:
Metallurgical and Materials Transactions A
DOI:
10.1007/s11661-016-3907-7
Date:
April, 2017
Fichier:
PDF, 2.37 MB
english, 2017