Homogeneous Microstructure of Bulk K4169 Superalloy Obtained by Stable Undercooling
Keren, Zhang, Faqin, Xie, Rui, Hu, Jinshan, Li, Xiangqing, WuVolume:
45
Langue:
english
Journal:
Rare Metal Materials and Engineering
DOI:
10.1016/s1875-5372(16)30055-8
Date:
February, 2016
Fichier:
PDF, 1.19 MB