Differential scanning calorimetry of phenol–formaldehyde resins cure-accelerated by carbonates
Byung-Dae Park, Bernard Riedl, Ernest W Hsu, Jack ShieldsVolume:
40
Année:
1999
Langue:
english
Pages:
11
DOI:
10.1016/s0032-3861(98)00400-5