Fractographic analysis of silkworm and spider silk
P Poza, J Pérez-Rigueiro, M Elices, J LLorcaVolume:
69
Année:
2002
Langue:
english
Pages:
14
DOI:
10.1016/s0013-7944(01)00120-5
Fichier:
PDF, 521 KB