Directional Solidification Behavior of CMSX-6 Superalloy
Zheng, Shuai, Jia, Yu Liang, Tang, JiaoVolume:
788
Langue:
english
Journal:
Materials Science Forum
DOI:
10.4028/www.scientific.net/MSF.788.554
Date:
April, 2014
Fichier:
PDF, 2.77 MB
english, 2014