New selector based on zinc oxide grown by low temperature atomic layer deposition for vertically stacked non-volatile memory devices
N. Huby, G. Tallarida, M. Kutrzeba, S. Ferrari, E. Guziewicz, Ł. Wachnicki, M. GodlewskiVolume:
85
Année:
2008
Langue:
english
Pages:
3
DOI:
10.1016/j.mee.2008.07.016
Fichier:
PDF, 341 KB
english, 2008