Effect of welding procedure on wear behaviour of a modified martensitic tool steel hardfacing deposit
Agustín Gualco, Hernán G. Svoboda, Estela S. Surian, Luis A. de VediaVolume:
31
Année:
2010
Langue:
english
Pages:
9
DOI:
10.1016/j.matdes.2010.04.026
Fichier:
PDF, 2.18 MB
english, 2010