Microstructures and fracture toughness of Ti–(43–48)Al–2Cr–2Nb prepared by electromagnetic cold crucible directional solidification
Wang, Yongzhe, Ding, Hongsheng, Zhang, Hailong, Chen, Ruirun, Guo, Jingjie, Fu, HengzhiVolume:
64
Langue:
english
Journal:
Materials & Design
DOI:
10.1016/j.matdes.2014.06.073
Date:
December, 2014