He and H irradiation effects on the nanoindentation hardness of CLAM steel
Jiang, Siben, Peng, Lei, Ge, Hongen, Huang, Qunying, Xin, Jingping, Zhao, ZiqiangVolume:
455
Langue:
english
Journal:
Journal of Nuclear Materials
DOI:
10.1016/j.jnucmat.2014.06.053
Date:
December, 2014