Modulated differential scanning calorimetry: 2. Studies of physical ageing in polystyrene
D.J. Hourston, M. Song, A. Hammiche, H.M. Pollock, M. ReadingVolume:
37
Année:
1996
Langue:
english
Pages:
5
DOI:
10.1016/0032-3861(96)81094-9
Fichier:
PDF, 555 KB
english, 1996