Effect of dissolved oxygen content on stress corrosion cracking of a cold worked 316L stainless steel in simulated pressurized water reactor primary water environment
Zhang, Litao, Wang, JianqiuVolume:
446
Langue:
english
Journal:
Journal of Nuclear Materials
DOI:
10.1016/j.jnucmat.2013.11.027
Date:
March, 2014
Fichier:
PDF, 7.61 MB
english, 2014