Fractal characteristics of stress corrosion cracking in SNCM 439 steel having different prior-austenite grain sizes
Masashi Kurose, Yukio Hirose, Toshihiko Sasaki, Yasuo YoshiokaVolume:
53
Année:
1996
Langue:
english
Pages:
10
DOI:
10.1016/0013-7944(94)00303-3
Fichier:
PDF, 515 KB
english, 1996