Stress corrosion cracking and pitting corrosion relation for zircaloy-4 in chloride-containing hydro-alcoholic media
Y. Roques, G. Mankowski, G. Chatainier, F. DabosiVolume:
32
Année:
1987
Langue:
english
Pages:
6
DOI:
10.1016/0013-4686(87)87092-5
Fichier:
PDF, 1.05 MB