Deformation behaviour of an advanced nickel-based superalloy studied by neutron diffraction and electron microscopy
Benedict M.B. Grant, Elisabeth M. Francis, Joao Quinta da Fonseca, Mark R. Daymond, Michael PreussVolume:
60