Differential scanning calorimetric study of poly(3-hydroxyoctanoate) inclusions in bacterial cells
Jae Jun Song, Sung Chul Yoon, Seungju M Yu, Robert W LenzVolume:
23
Année:
1998
Langue:
english
DOI:
10.1016/s0141-8130(98)00046-4