Differential Scanning Calorimetry (DSC) for Interdiffusion Studies in PVC/PnBMA Blend: A Quantitative Analysis
Günter Dlubek, Gisela Pompe, Jürgen Pionteck, Andreas Janke, Duncan KilburnVolume:
204
Année:
2003
Langue:
english
Pages:
11
DOI:
10.1002/macp.200390093
Fichier:
PDF, 326 KB
english, 2003