Environmental and internal hydrogen embrittlement of a directionally solidified Ni-rich Ni3AI intermetallics
Jian-Qing Su, Shu-Jun Gao, Zhuang-Qi HuVolume:
35
Langue:
english
Pages:
6
DOI:
10.1023/a:1004783519661
Date:
March, 2000
Fichier:
PDF, 948 KB
english, 2000